CA9 – CE9 TEST RESULTS 2

Damp heat
CA9 Through-hole and SMD500 h. at 40°C and 95% RH
CE9 Through-hole and SMD+5%, -2%
500 h. at 40°C and 95% RH
±2%
Thermal cycles
CA9 Through-hole and SMD16 h at 85ºC, plus 2 h at –25ºC
CE9 Through-hole and SMD±2.5%
16 h at 90ºC, plus 2 h at –40ºC
±2%
Load life
CA9 Through-hole and SMD1.000 h. at 50°C
CE9 Through-hole and SMD+0%; -6%
1.000 h. at 70°C
±2%
Mechanical life
CA9 Through-hole and SMD1.000 cycles at 10 c.p.m.and at 23°C ± 2°C
CE9 Through-hole and SMD±3%
1.000 cycles at 10 c.p.m. and at 23°C ± 2°C
±3%
Storage (3years)
CA9 Through-hole and SMD3 years at 23°C ± 2°C
CE9 Through-hole and SMD±3%
3 years at 23°C ± 2°C
±1%
CA9 Through-hole and SMD CE9 Through-hole and SMD
Damp heat 500 h. at 40°C and 95% RH +5%, -2% 500 h. at 40°C and 95% RH ±2%
Thermal cycles 16 h at 85ºC, plus 2 h at –25ºC ±2.5% 16 h at 90ºC, plus 2 h at –40ºC ±2%
Load life 1.000 h. at 50°C +0%; -6% 1.000 h. at 70°C ±2%
Mechanical life 1.000 cycles at 10 c.p.m.and at 23°C ± 2°C ±3% 1.000 cycles at 10 c.p.m. and at 23°C ± 2°C ±3%
Storage (3years) 3 years at 23°C ± 2°C ±3% 3 years at 23°C ± 2°C ±1%